TIG welding rod size (steel)

by Ignoramus26857 <ignoramus26857@[EMAIL PROTECTED] > Oct 27, 2008 at 12:24 AM

For regular kinds of TIG welding jobs, such as not too thick steel,
would you say that 3/32 is better than 1/8? I need to order some more
rod and I have never tried 1/8" size. 

-- 
   Due to extreme spam originating from Google Groups, and their
inattention 
      to spammers, I and many others block all articles originating 
       from Google Groups. If you want your postings to be seen by 
         more readers you will need to find a different means of 
                       posting on Usenet.
                   http://improve-usenet.org/
 




 15 Posts in Topic:
TIG welding rod size (steel)
Ignoramus26857 <ignora  2008-10-27 00:24:54 
Re: TIG welding rod size (steel)
Ernie Leimkuhler <erni  2008-10-27 03:19:59 
Re: TIG welding rod size (steel)
TinLizziedl <nothere@[  2008-10-27 20:08:27 
Re: TIG welding rod size (steel)
"Pete C." <a  2008-10-27 22:46:05 
Re: TIG welding rod size (steel)
Ignoramus13094 <ignora  2008-10-27 23:16:29 
Re: TIG welding rod size (steel)
BobH <WanderingMetalHe  2008-10-28 04:24:39 
Re: TIG welding rod size (steel)
matthew maguire <matth  2008-11-08 10:31:51 
Re: TIG welding rod size (steel)
Ernie Leimkuhler <erni  2008-11-08 14:08:44 
Re: TIG welding rod size (steel)
"SteveB" <to  2008-11-08 19:13:40 
Re: TIG welding rod size (steel)
matthew maguire <matth  2008-11-09 06:27:20 
Re: TIG welding rod size (steel)
"Watson" <sa  2008-11-10 23:15:44 
Re: TIG welding rod size (steel)
Ernie Leimkuhler <erni  2008-11-10 23:05:35 
Re: TIG welding rod size (steel)
matthew maguire <matth  2008-11-17 07:31:49 
Re: TIG welding rod size (steel)
Ernie Leimkuhler <erni  2008-11-17 20:47:54 
Re: TIG welding rod size (steel)
erngineman <engineman1  2008-11-10 12:59:24 

Post A Reply:
  Go here to Signup

AddThis Feed Button


About - Advertising - Contact - Frequently Asked Questions - Privacy Policy - Terms of Use - Signup

Contact
localhost-V2008-12-19 Fri Jan 9 14:10:22 PST 2009.