Pictures -- was Can a hard bearing ball be welded to mild steel

by Ignoramus20172 <ignoramus20172@[EMAIL PROTECTED] > Oct 28, 2008 at 11:57 PM

On 2008-10-29, Gunner Asch <gunner@[EMAIL PROTECTED]
> wrote:
> Tig works nicely, as does brazing and even mig and stick
>
> Tig would be prettier
>

Here's the end result with TIG.

http://igor.chudov.com/projects/Welding/17-Vise-Handle-With-Bearing-Balls/

-- 
   Due to extreme spam originating from Google Groups, and their
inattention 
      to spammers, I and many others block all articles originating 
       from Google Groups. If you want your postings to be seen by 
         more readers you will need to find a different means of 
                       posting on Usenet.
                   http://improve-usenet.org/
 




 7 Posts in Topic:
Pictures -- was Can a hard bearing ball be welded to mild steel
Ignoramus20172 <ignora  2008-10-28 23:57:15 
Re: Pictures -- was Can a hard bearing ball be welded to mild st
"Buerste" <B  2008-10-29 01:49:56 
Re: Pictures -- was Can a hard bearing ball be welded to mild st
Jman <mooglieman@[EMAI  2008-10-29 10:45:55 
Re: Pictures -- was Can a hard bearing ball be welded to mild st
Jeff Wisnia <jwisnia@[  2008-10-30 11:30:07 
Re: Pictures -- was Can a hard bearing ball be welded to mild st
"Lloyd E. Sponenburg  2008-10-30 10:47:45 
Re: Pictures -- was Can a hard bearing ball be welded to mild st
Ignoramus11000 <ignora  2008-10-30 12:31:59 
Re: Pictures -- was Can a hard bearing ball be welded to mild st
Ignoramus11000 <ignora  2008-10-30 12:30:51 

Post A Reply:
  Go here to Signup

AddThis Feed Button


About - Advertising - Contact - Frequently Asked Questions - Privacy Policy - Terms of Use - Signup

Contact
localhost-V2008-12-19 Fri Jan 9 15:55:15 PST 2009.