Need SS filler recommendation...

by "Pete C." <aux3.DOH.4@[EMAIL PROTECTED] > Oct 30, 2008 at 05:10 PM

I have acquired some stainless SCUBA tank clamp bands that were made for
tanks a bit larger than the typical 80CF aluminum cylinders. I need to
cut them down and reweld them to use on my 80CF tanks. The SS alloy of
the bands is unknown. I need a recommendation on what SS filler to use
for TIGing them back together. I don't have any SS filler on hand, so I
have to go shopping no matter what the recommendation is.

Thanks,

	Pete C.
 




 2 Posts in Topic:
Need SS filler recommendation...
"Pete C." <a  2008-10-30 17:10:27 
Re: Need SS filler recommendation...
Ernie Leimkuhler <erni  2008-10-30 19:34:58 

Post A Reply:
  Go here to Signup

AddThis Feed Button


About - Advertising - Contact - Frequently Asked Questions - Privacy Policy - Terms of Use - Signup

Contact
localhost-V2008-12-19 Fri Jan 9 14:02:52 PST 2009.