by "justme" <jbleaux@[EMAIL PROTECTED] > Nov 5, 2008 at 09:19 PM

The traveling nut on my vise broke and I need to weld it back together with

high-nickle rods.  I have already ground it so as to take more weld
filler. 
However, how do I ensure that the tlreads don't take filler?

Thanks
 




 9 Posts in Topic:
How to Weld cast iron with internal thread
"justme" <jb  2008-11-05 21:19:38 
Re: How to Weld cast iron with internal thread
Ignoramus31261 <ignora  2008-11-05 21:21:02 
Re: How to Weld cast iron with internal thread
Bruce in Bangkok <decy  2008-11-06 11:55:54 
Re: How to Weld cast iron with internal thread
Bruce in Bangkok <decy  2008-11-06 11:54:50 
Re: How to Weld cast iron with internal thread
dcaster@[EMAIL PROTECTED]  2008-11-05 21:03:36 
Re: How to Weld cast iron with internal thread
"fran...123" &l  2008-11-06 10:57:19 
Re: How to Weld cast iron with internal thread
Peter Fairbrother <zen  2008-11-06 20:47:56 
Re: How to Weld cast iron with internal thread
"Leo Lichtman"   2008-11-06 20:59:01 
Re: How to Weld cast iron with internal thread
"justme" <jb  2008-11-06 18:41:19 

Post A Reply:
  Go here to Signup

AddThis Feed Button


About - Advertising - Contact - Frequently Asked Questions - Privacy Policy - Terms of Use - Signup

Contact
localhost-V2008-12-19 Fri Jan 9 15:19:43 PST 2009.